If you can't view the Datasheet, Please click here to try to view without PDF Reader . |
|
Datasheet File OCR Text: |
OS-CON DATA SHEET OS-CON 16SVP82M Frequency (kHz) Impedance (ohm) ESR (ohm) 0.12 16.81 0.22 0.5 4.08 0.11 1 2.05 0.08 10 0.223 0.048 100 0.041 0.032 500 0.025 0.024 1000 0.031 0.025 5000 0.111 0.025 10000 0.192 0.025 No.OS02N-DFSVP028 Frequency characteristics 1000 100 Impedance (ohm) ESR (ohm) ESR, Impedance (ohm) 10 1 0.1 0.01 0.001 0.1 1 10 100 1000 10000 Frequency (kHz) Measuring equipment: HP4194A Test fixture: HP16047C Measuring position: root of leads OS Engineering Department, OS-CON Control Department Saga SANYO Industries Co., Ltd. n = 3p.(Ave.) Room temperature OS-CON DATA SHEET SVP series Test item Endurance (After V.P.S test) Test temperature 105 deg.C Applied voltage 16 V Model 16SVP82M Lot No. 030202151 Change in capacitance (120Hz) 20 10 0.15 0.14 0.13 0.12 0.11 0.1 0.09 0.08 0.07 0.06 0.05 0.04 0.03 0.02 0.01 0 Tangent of loss angle (120Hz) 0 -10 -20 -30 -40 0 2000 Tangent of loss angle Percent delta [%] 0 2000 Time[h] Time[h] ESR (100kHz) 100 90 80 70 60 50 40 30 20 10 0 10000 Leakage current (16V 60s) Leakage current(A) 1000 100 10 1 0.1 0.01 ESR(mohm) 0 2000 0 2000 Time[h] Time[h] Note: n =30p. (V.P.S = Vapor Phase Soldering method) Note: V.P.S test conditions : 230deg.Cx75sx2times Start on March 29, 2000 Executed by M. Koyama End on June 21, 2000 Drawn by S. Kodera No.OS02D-DESVP028 OS Engineering Department., OS-CON Control Department, Saga SANYO Industries Co., Ltd. OS-CON DATA SHEET SVP series Test item Damp heat (Steady state) (After V.P.S test) Test temperature 60 deg.C Test humidity 90% RH Model 16SVP82M Lot No. 030202151 Change in capacitance (120Hz) 20 10 0.15 0.14 0.13 0.12 0.11 0.1 0.09 0.08 0.07 0.06 0.05 0.04 0.03 0.02 0.01 0 Tangent of loss angle (120Hz) Tangent of loss angle Percent delta [%] 0 -10 -20 -30 -40 0 1000 0 1000 Time[h] Time[h] ESR (100kHz) 100 90 80 70 60 50 40 30 20 10 0 10000 Leakage current (16V 60s) Leakage current(A) 0 1000 1000 100 10 1 0.1 0.01 ESR(mohm) 0 1000 * Time[h] Time[h] Note: n =20p. (V.P.S = Vapor Phase Soldering method) Note: V.P.S test conditions : 230deg.Cx75sx2times *Voltage Processing: Applying rated voltage for 120s at 105deg.C. Start on March 29, 2000 Executed by M. Koyama End on May 9, 2000 Drawn by S. Kodera No.OS02D-DHSVP028 OS Engineering Department, OS-CON Control Department, Saga SANYO Industries Co., Ltd. |
Price & Availability of 16SVP82M
![]() |
|
|
All Rights Reserved © IC-ON-LINE 2003 - 2022 |
[Add Bookmark] [Contact Us] [Link exchange] [Privacy policy] |
Mirror Sites : [www.datasheet.hk]
[www.maxim4u.com] [www.ic-on-line.cn]
[www.ic-on-line.com] [www.ic-on-line.net]
[www.alldatasheet.com.cn]
[www.gdcy.com]
[www.gdcy.net] |